E44-1104 · Other · Rubber Hose · ★★
Aged, leaking, seeping.
[Mechanism] The hose material was not resistant to the medium and was past its service life; the rubber aged, cracked, and seeped.
[Calculation] Hose in service 3 years (should be ≤2); aging dropped burst pressure from 4MPa to 1.5MPa; working pressure 1.0MPa left insufficient margin, causing seepage.
[Design Omission] No medium-resistant hose selection, no replacement interval, no protective sleeve, and no pressure test.
1) Choose a medium-resistant hose (fluororubber replacing ordinary); aging leaks, and resistant material seals, restoring tightness;
2) Set a replacement interval ≤2 years (was 3); long service leaks, and controlled intervals replace it, preventing leakage;
3) Add a protective sleeve (against abrasion and puncture); abrasion leaks, and a sleeve protects, extending life;
4) Control temperature ≤80℃ (against aging); high temperature ages, and temperature control protects, suppressing aging;
5) Run a pressure test (hold at 1.5× working pressure); untested means unknown, and measured tightness confirms it;
6) Install seepage monitoring (alarm on wetness); a leak first shows as seepage, and early warning catches it;
7) Prevent offset stress (lay straight); offset leaks, and straight laying evens the load;
8) Record hose selection and replacement interval in the hose specification; the root cause of leakage was non-resistant material and over-service, so the specification must gate it.
GB/T 10544-2013 Rubber hoses