Internal Scaling Increases Pipe Resistance

E44-1026 · Excessive Piping Resistance & Pressure Drop · Piping · ★★

Problem Symptom

Scaling, resistance rising, pressure drop

Root Cause

[Mechanism] Scaling inside the pipe increases the absolute roughness epsilon, raises the friction factor, and the flow decays year by year.
[Calculation] Originally epsilon=0.05mm; after 3 years of scaling epsilon=1.5mm, lambda rose from 0.019 to 0.038, the flow at the same valve position fell 22% and hf doubled.
[Design Omission] The line was never pigged, no corrosion or scale inhibitor was added, and the wall thickness was never inspected.

Correct Solution

1) Pig the line mechanically (PIG ball, descaling to epsilon<=0.1mm); 3 years of scaling raised epsilon from 0.05 to 1.5mm and doubled lambda, and cleaning lowers the roughness so the flow returns to the design value;
2) Verify the roughness epsilon and lambda (using the Colebrook equation); a large epsilon raises lambda and the check quantifies it;
3) Add a corrosion and scale inhibitor (inhibition efficiency >=85%); scaling raises the resistance and the inhibitor suppresses it, preventing the roughness from rising;
4) Raise the pump head with a 25% margin (to cover the scaled resistance); a rising resistance leaves the terminal under-pressurised and raising the head compensates, securing the flow;
5) Carry out a resistance test (compare DeltaP before and after cleaning); without the test the effect of scaling is unknown, so measurement validates it and the data fixes the resistance;
6) Control the turbidity of the medium to <=50mg/L (upstream filtration); turbidity causes scaling and controlling it slows the effect, preventing scale;
7) Fit an online flow meter (report and pig when the deviation exceeds 10%); scaling shows up first as a flow drop and early reporting leads to cleaning, monitoring the resistance;
8) Write the pigging and the epsilon verification into the specification; the root cause of the scaling was a missing cleaning routine with no scale inhibitor, so the specification closes the loop.

Checklist

References

GB/T 20801.3-2020 Design Code for Industrial Metallic Piping

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »