E44-057 · Valve Selection and Internal Leakage · Globe Valve · ★★
Solids and particles erode the seat sealing face; internal leakage is 2.5L/min (should be ≤0.1), and the valve won't shut tight, needing a bypass to relieve
[Mechanism] High-velocity particles scour the sealing face, raising roughness and breaking the line contact.
[Calculation] Particle size beyond what the seating pressure tolerates presses 0.2mm-deep marks; leakage ΔQ∝gap³ rises tens of times.
[Design Omission] No wear-resistant seat chosen and no upstream strainer - internal leakage followed.
1) Hardface the seat or switch to a metal-to-metal seal (e.g. Stellite), since high-velocity particles roughened the soft face and broke line contact, giving an erosion-resistant hard face that holds seating pressure;
2) Fit an upstream strainer to hold particle size ≤ the seal gap, since oversize grains press 0.2mm marks and raise leakage ΔQ∝gap³, cutting the erosion source at the start;
3) Lower the medium velocity into a sensible range, since particle kinetic energy ∝v² and scouring worsens at high v, slowing flow to ease erosion;
4) Periodically lap the sealing faces to restore flatness, since erosion pits them and they won't seal, maintaining line contact and returning leakage to ≤0.1L/min;
5) Fit online leak detection (downstream flow or acoustics), since internal leakage is gradual and hard to spot, giving early alarm to avoid bypass relief spreading;
6) Add a valve-body drain to route leakage to a sump, so any internal leakage of liquid medium can be collected, keeping the downstream clean and enabling leak metering;
7) Accept leakage ≤0.1L/min at commissioning, since the standard is a quantitative criterion and poor shutoff needs measurement, accepting on data;
8) Put wear-resistant selection into the medium-adaptation spec, since particle service wrongly used a soft seat, fixing the seal type by medium characteristics at selection stage.
GB/T 12235-2007 Steel globe valves for petrochemical industry