E44-272 · Valve Selection and Internal Leakage · Bellows globe valve WJ41H-16P DN40 · ★★★
After 120,000 cycles the weld seam cracked and leaked externally, and the medium seeped into the stem cavity; service life was only 8 months.
[Fatigue] The bellows stretches axially on each stroke; the stress amplitude exceeded the endurance limit and cracked the weld.
[Creep] High temperature made the bellows material creep and thin the wall.
[Design Omission] No control of cycle count or temperature, and no multi-layer bellows chosen — the bellows valve cracked.
1) Select a multi-layer bellows (≥3 plies) by cycle count; a single ply cracked at 120,000 cycles with 8-month life, so use multi-ply for fatigue strength;
2) Limit stroking frequency and reduce stroke shock; frequent stroking pushes the stress amplitude over the limit, so slow it down to extend life;
3) At high temperature, lower the wall temperature or switch to a heat-resistant alloy; heat thins the wall by creep, so make it temperature-resistant;
4) Radiograph the weld seams; cracks start at weld defects, so inspect the welds;
5) Add a leak-detection hole in the stem cavity for early notice; cracks grow and leak out, so make it detectable;
6) Replace the bellows on a cycle-based schedule; fatigue has a finite life, so replace on schedule;
7) Switch to a low-fatigue bellows profile; the profile affects the stress amplitude, so optimize the form;
8) Write the cycle life into the design; the lack of control was the cause of cracking, so gate it at design.
GB/T 12722-2008 General technical specification for bellows expansion joints