E44-288 · Valve Selection and Internal Leakage · High-temperature bellows globe valve WJ41H-25P DN40 · ★★★
At 350℃ the bellows crept and lost spring tension; the stem loosened and leaked externally, still leaking after being tightened twice a month.
[Creep] High temperature makes the bellows material creep, stiffness drops, and the sealing load is lost.
[Leak] With spring tension gone, the medium leaks out along the stem clearance.
[Design Omission] No heat-resistant bellows and no disc-spring compensation were chosen — the high-temperature valve leaked.
1) Choose a heat-resistant bellows such as Inconel; the original crept and lost tension at 350℃ and leaked at the loose stem, so make it temperature-resistant;
2) Add a disc spring to compensate for creep and hold the sealing load; creep loses the spring load, so keep constant load;
3) Fit heat sink fins on the stem to lower the bellows temperature; heat is the source of creep, so cool it;
4) Retighten hot on a marked schedule; creep keeps loosening it, so tighten to the mark;
5) Switch to a metal-hard-seal stem; hard faces do not creep, so make it durable;
6) Add a leak alarm; external leakage is hazardous, so make it controlled;
7) Keep the service temperature within the allowable rating; over-temperature speeds creep, so control the temperature;
8) Write heat resistance and compensation into the design; the missing provisions were the cause of leakage, so gate it at design.
GB/T 12722-2008 General technical specification for bellows expansion joints