E44-060 · Seal Leakage · Pump Mechanical Seal · ★★
The stationary-ring O-ring aged and hardened from long heat exposure, leaking 3 drops/min at the seal (should be zero), with seepage at the shaft seal.
[Aging] The O-ring ages under heat, hardening and losing elasticity, so its compression rebound is insufficient.
[Calculation] The operating temperature exceeds the O-ring rating, dropping compression from 15% to 6% — below the 8% needed to seal, so the seal fails.
[Design Omission] The O-ring material was not chosen for the medium temperature and no drain recovery was set — it leaked.
1) Change the O-ring to heat-resistant FKM or FFKM; the original ring aged and hardened, losing elasticity, dropping compression from 15% to 6% below the 8% seal requirement, so restore rebound and face contact;
2) Keep the seal-chamber temperature within the material rating (add flush or cooling); temperature is the main aging driver and controlling it extends life, so remove the failure at the source;
3) Add a drain sump to recover seepage; once leaked, liquid medium can be collected without polluting the environment, and leakage volume can be tracked;
4) Check the spring face pressure is in the design band; too low opens the faces, too high wears fast, so hold a reasonable pressure to extend life;
5) Replace O-rings periodically (by temperature life); aging is irreversible and planned parts replacement prevents sudden failure, so use scheduled overhaul instead of breakdown downtime;
6) Add leak collection and alarm; dripping is gradual and needs monitoring, so detect it early before shaft-seal failure spreads;
7) Run a trial test for no dripping; the seal's job is zero leakage and it needs actual measurement, so make it acceptance;
8) Bring material temperature into seal selection; the O-ring material was not chosen by medium temperature, so check temperature at the selection stage.
GB/T 14211-2018 Mechanical seals - Test methods