Packing Swollen by the Medium Causes Leakage

E44-560 · Seal Leakage · Acid and Alkali Pump Packing · ★★

Problem Symptom

Packing swells and jams, leaks 1L/h, volume increase 30%

Root Cause

[Mechanism] The packing is not resistant to the medium and swells.
[Calculation] The 30% swell makes the packing jam, the clearance becomes uneven and it leaks.
[Design Omission] Corrosion-resistant packing was not selected, no test was performed, and no material grading was done - the material was simply wrong.

Correct Solution

1) Change to corrosion-resistant packing (PTFE-impregnated graphite, resistant from pH 0 to 14); the original packing was incompatible with the acid and alkali, absorbed liquid, swelled 30% in volume, jammed, lost its rebound and leaked 1L/h, so corrosion-resistant non-swelling packing keeps its rebound and stops the leak;
2) Carry out a media compatibility test (72h immersion with a volume change of <=5%); without the test the wrong material is selected and the packing swells and jams, so testing first settles the material;
3) Control the medium concentration at <=30% (dilute or match the material); a high concentration promotes molecular swelling and controlling the concentration reduces the swelling;
4) Use different materials by section (PTFE in the corrosive section, graphite in the clean section); using one material for the whole pump causes swelling of the wrong material, so selecting per section matches the duty;
5) Leave a 2mm swell gap (allow for the packing box depth); swelling causes the shaft to jam and the gap accommodates the swelling;
6) Reduce the working temperature (<=80C); a temperature rise accelerates molecular swelling and cooling reduces the swelling;
7) Set a swell inspection interval (every 3 months, measure with a caliper); gradual swelling causes jamming and leakage, so inspection leads to replacement;
8) Write the corrosion-resistant packing into the specification; the original omission of material selection was the root cause of the swelling, so the specification closes the loop.

Checklist

References

GB/T 12224-2015 Steel Valves