E44-561 · Seal Leakage · Steam Flange DN80 · ★★★
Flange leaks, gasket at 300C exceeds its 200C rating, gasket blown out
[Mechanism] The gasket is not resistant to the temperature and pressure and is blown out by the medium.
[Calculation] The temperature 300C exceeds 200C and the pressure 1.6MPa exceeds 1.0MPa, so the gasket is blown out.
[Design Omission] No temperature/pressure class was selected, the parameters were not verified, and no test was performed - the wrong gasket was fitted.
1) Change to a high-temperature gasket (spiral-wound metal with flexible graphite, resistant to 600C, suitable for PN16/1.6MPa); the original non-metallic gasket degraded and lost its rebound at 300C above its 200C rating, and the system pressure of 1.6MPa above the rated 1.0MPa blew the gasket out of the joint, so a temperature- and pressure-resistant gasket is not blown out and restores the seal;
2) Verify the temperature/pressure class (flange PN16 matched to the 1.6MPa duty); the gasket pressure class being below the actual 1.6MPa is the direct cause of the blow-out, so verifying the class eliminates the over-pressure blow-out;
3) Select a thicker gasket for more rebound (3mm spiral-wound); a thin gasket has insufficient specific pressure under preload and is easily blown out by high-velocity steam, so thickening it increases the preload resilience against blow-out;
4) Control the temperature at <=250C (reduce temperature and pressure or change material); above 200C the non-metallic gasket degrades and the 300C steam is the trigger, so cooling brings the duty inside the gasket rating;
5) Reduce the working pressure to 1.0MPa (or upgrade the flange to PN25); 1.6MPa above 1.0MPa blows the gasket out, so lowering the pressure or upgrading the flange removes the over-pressure condition;
6) Carry out a gasket temperature and pressure test (1.5 times the design pressure, hot-tightened at 300C); without the test the blow-out incident happened, so testing first proves the selection;
7) Set a routine gasket condition inspection (dye-penetrant check at every major overhaul); gradual thermal degradation causes leakage, so inspection leads to replacement;
8) Write the temperature and pressure class into the piping specification; the original omission of a pressure and temperature class was the root cause of the blow-out, so the specification closes the loop.
HG/T 20606-2017 Non-Metallic Gaskets for Steel Pipe Flanges