E44-567 · Seal Leakage · Globe Valve DN50 · ★★
Stem leakage, 8 drops/min, packing hard
[Mechanism] Stem wear combined with a hard packing causes the leakage.
[Calculation] The stem Ra1.6 against 0.8 and the hard packing leave a gap that leaks.
[Design Omission] A soft packing was not selected, the stem was not polished, and the gland was not tightened - the joint leaked.
1) Polish the stem to Ra0.8 (lapping compound); the original Ra1.6 and the 8 drops/min left a stem-to-packing gap that leaked, and reducing the roughness to 0.8 stops the dripping;
2) Change to a soft packing (flexible graphite, rebound >40%); a hard packing cannot fill the micro-gap on the stem, so a soft packing conforms to the stem;
3) Tighten the gland to a packing pressure of 0.1MPa (torque); a loose gland leaves a gap that leaks, so tightening the gland compacts the packing;
4) Add packing sealing grease (graphite grease); a dry gap lets the medium seep straight through, so grease fills the gap;
5) Control the stem runout to <=0.05mm (bearings and guide); a wandering stem wears and leaks, and controlling the runout protects it;
6) Select a wear-resistant packing (with molybdenum disulphide); a worn stem creates the gap, so a wear-resistant packing copes with it;
7) Set a routine drip count check (every shift); the leak develops gradually into dripping, so the drips are counted;
8) Write the polishing and the soft packing into the maintenance card; the original failure to select the material was the root cause of the leakage, so the maintenance card closes the loop.
GB/T 12224-2015 Steel Valves