E44-588 · Seal Leakage · Bellows Compensator · ★★★
Leakage, two bellows cracks
[Mechanism] The bellows fails by fatigue.
[Calculation] Thousands of cycles cause the crack.
[Design Omission] The fatigue life was never verified, the travel was not limited and nothing was inspected - the bellows cracked.
1) Verify the fatigue life against the design cycle count (per EJMA, based on the travel cycle); the original two cracks were the result of exceeding the fatigue limit, and verifying the life extends it;
2) Limit the travel to +/-20mm (guides and limit stops); exceeding it cracks the bellows, and limiting it prevents that;
3) Change to a thicker-walled compensator (wall thickness increased by 0.5mm); a thin wall cracks easily, and thickening it prevents cracking;
4) Add guide supports to prevent misalignment (avoiding rubbing); misalignment cracks the bellows, and guiding it prevents that;
5) Control the rate of temperature change (change slowly); a rapid change cracks it, and controlling the rate prevents that;
6) Inspect the bellows wall thickness (thickness measurement); it thins gradually and then cracks, so the thickness is inspected;
7) Avoid water hammer (venting and slow opening); a surge cracks the bellows, and avoiding it prevents that;
8) Write the fatigue verification and the travel limit into the specification; the original failure to verify the fatigue life was the root cause of the cracking, so the specification closes the loop.
GB/T 12777-2019 Metal Bellows Expansion Joints