E44-591 · Seal Leakage · Shell-and-Tube Heat Exchanger Nozzle · ★★★
Leakage, weld crack
[Mechanism] The nozzle weld was not fully penetrated and cracked.
[Calculation] The lack of penetration caused the leak.
[Design Omission] The weld was not fully penetrated, not inspected and not tested - the joint cracked.
1) Reweld the nozzle with full penetration (tig root pass plus cap pass); the original incomplete penetration and heat cracking leaked, and full penetration stops the leak;
2) Carry out a radiographic weld inspection (RT); without inspection the crack stayed and it leaked, so the weld is inspected;
3) Carry out a pneumatic leak test (shell side 0.1MPa); without the test the leak went undetected, so the test confirms tightness;
4) Select a matching filler wire (same base material); a dissimilar material cracks, and matching materials prevent that;
5) Control the weld heat to prevent distortion (symmetrical segmented welding); distortion under a changing duty causes cracking, and controlling the heat prevents it;
6) Grind the root and remove slag (back gouging); slag causes cracking, and cleaning the root prevents it;
7) Set a routine weld inspection (RT or PT at every overhaul); cracks develop gradually and then leak, so the weld is inspected;
8) Write the full penetration and the leak test into the welding card; the original failure to weld was the root cause of the leak, so the welding card closes the loop.
GB/T 151-2014 Heat Exchangers