E44-590 · Seal Leakage · Cooler Tube Sheet · ★★
Leakage, expanded tube joint loose
[Mechanism] Insufficient expansion makes the joint loose.
[Calculation] An insufficient expansion rate makes the joint loose and it leaks.
[Design Omission] The expansion rate was not controlled, nothing was inspected and the joint was not re-expanded - it stayed loose.
1) Re-expand to an expansion rate of 8% (rolling plus strength expansion); the original insufficient expansion rate left the tube-to-sheet joint loose and leaking, and sufficient expansion stops the leak;
2) Control the expansion rate by test (expand a sample tube); without control the joint stayed loose, so the rate is controlled;
3) Inspect the expanded joint by leak test (ammonia or hydrostatic test); without inspection it leaked, so the joint is tested;
4) Select a matching tube diameter for the sheet (tolerance fit); a mismatch leaves it loose, and the correct fit prevents that;
5) Clean the tube bore and remove rust (sand blasting); rust prevents a tight fit, and cleaning the bore prevents it;
6) Repair-weld the loose joint (expand plus weld); the expansion was insufficient, and weld repair makes the joint permanent;
7) Set a routine inspection of the expanded joints (at every major overhaul); the joint loosens gradually and then leaks, so it is inspected;
8) Write the expansion rate control and the leak test into the assembly card; the original absence of expansion control was the root cause of the looseness, so the assembly card closes the loop.
GB/T 151-2014 Heat Exchangers