E44-465 · Filter Clogging and Contamination · Ceramic Element 1μm · ★★
During high-temperature regeneration firing, heating/cooling ramped too fast, elements cracked thermally, integrity dropped from 100% to 70%, and particles leaked at the outlet.
[Mechanism] Rapid heating creates a thermal-stress gradient between inside and outside of the ceramic that exceeds its flexural strength, causing cracking.
[Calculation] At a ramp >50℃/min, ΔT=200℃, thermal stress σ=EαΔT exceeds flexural strength, and the crack rate is 30%.
[Design Omission] No heating/cooling ramp control was set for regeneration; bare firing caused cracking.
1) Limit regeneration heating/cooling ramps to ≤10℃/min, because the original >50, ΔT=200, σ exceeded strength and cracking was 30%, thereby ramping slowly to prevent cracking;
2) Arrange uniform hot-air ports in the furnace to prevent localized heating, because local heat cracks, thereby equalizing temperature;
3) Air-dry naturally before firing against steam explosion, because wet elements explode, thereby drying;
4) Perform a bubble leak test after regeneration, because cracks leak and lower integrity, thereby leak-testing;
5) Sort out cracked elements separately, because they leak particles, thereby rejecting cracked ones;
6) Hold firing temperature within material limits, because exceeding it damages the material, thereby controlling temperature;
7) Support elements on cushioned brackets against mechanical shock, because vibration promotes cracking, thereby cushioning support;
8) Write heating/cooling ramps into the regeneration card, because the original uncontrolled ramp is the root cause of cracking, thereby enforcing regeneration control.
GB/T 13554-2020 High-efficiency air filters