E44-482 · Filter Clogging and Contamination · Gas Filter Glass-Fiber Paper · ★★
High-humidity gas weakened the wet filter paper, it burst through, and outlet dust reached 5mg>1mg
[Mechanism] Moisture weakened the interlayer bond of the glass fiber paper, and differential pressure burst it.
[Calculation] Moisture content >5% reduced tensile strength 40%; Δp=1kPa burst the paper, and bypass dust reached 5mg.
[Design Omission] No preheating to remove water and no moisture protection, so the paper burst.
1) Preheat the inlet gas above the dew point; since moisture >5% cut tensile strength 40% and caused the burst, preheating prevents moisture damage;
2) Add dehumidification upstream of the filter; since moisture damages the paper, dehumidification protects it;
3) Switch to water-resistant treated filter paper; since the plain paper absorbed moisture, water-resistant paper prevents it;
4) Monitor outlet dust content; since a burst is detectable, dust monitoring catches it;
5) Add a Δp alarm to prevent overpressure; since overpressure bursts the paper, the alarm warns;
6) Insulate the housing to prevent condensation; since condensation causes moisture, insulation prevents it;
7) Inspect paper strength periodically; since moisture damage develops gradually, inspection tracks it;
8) Write moisture protection into the gas-filter procedure; since the paper was never protected, the root cause of moisture damage, the gas-filter procedure provides the check.