Packing debris enters the circulating water and clogs the mesh, Δp=0.1MPa, heat transfer drops
[Mechanism] Packing ages and breaks into fragments that lodge in the mesh with the water.
[Calculation] Debris length > mesh opening, 35% of openings bridged, v rises, Δp=0.1.
[Design Omission] No upstream coarse strainer and aged packing; debris blockage results.
1) Add a coarse strainer upstream to catch debris, because the original 35% bridging and Δp=0.1 caused the blockage, so coarse straining keeps flow clear;
2) Replace packing on schedule to prevent aging breakage, because aged packing fragments, so scheduled replacement is used;
3) Make the mesh backwashable, because buildup blocks it, so backwashing is used;
4) Set a Δp alarm, because over-limit lowers performance, so an alarm is provided;
5) Side-stream filter the circulating water to reduce load, because the load is high, so side-stream filtration is used;
6) Monitor debris quantity, because a high count signals aging, so debris is monitored;
7) Make inlet and outlet the same size for easy inspection, because inspection was difficult, so inspection is made easy;
8) Write coarse straining and packing replacement into the cooling-tower specification, because the lack of coarse straining was the root cause of debris, so the tower spec governs.