E44-508 · Heat Exchanger Fouling and Insufficient Heat Transfer · Condenser Copper Tube · ★★
Copper-tube scaling, vacuum drop, coal-consumption rise
[Mechanism] Circulating-water scale deposits on the copper tubes.
[Calculation] Rf=0.4 cuts K by 35%, drops vacuum by 0.008, and raises coal consumption by 2%.
[Design Omission] No scale inhibitor and no rubber-ball cleaning, so scaling occurs.
1) Dose scale inhibitor and run continuous rubber-ball cleaning (ball recovery rate ≥95%); circulating water scales the copper tubes (Rf=0.4, K drop 35%, vacuum drop 0.008, coal +2%), so inhibitor and ball cleaning restore K and vacuum and cut consumption;
2) Stabilize circulating water (control pH / hardness, concentration ratio ≤3); unstable water promotes scale, so water stabilization suppresses deposition;
3) Monitor vacuum (alarm when vacuum falls 0.005 below design); scaling shows up first as vacuum drop, ahead of the coal-consumption rise, so vacuum monitoring gives early warning;
4) Inspect copper-tube thickness on schedule (measure scale / wall thickness every two years); scaling and corrosion worsen K drop and vacuum loss, so quantitative data guides cleaning;
5) Raise flow velocity to prevent settling (≥1.2 m/s); scale settles in low-velocity zones, so higher velocity reduces residence time and suppresses settling;
6) Disinfect to prevent slime (oxidizing biocide); bacteria and algae slime promote scaling, so disinfection suppresses adhesion;
7) Fit a terminal-temperature-difference alarm (alarm when terminal difference > design +5℃); scaling first raises the terminal difference as a scale indicator, so monitoring it gives early warning;
8) Write inhibitor and rubber-ball cleaning into the condenser procedure; the original design omitted inhibitor and ball cleaning, the root cause of scaling, so the procedure closes the loop.
GB/T 151-2014 Heat exchangers