E44-509 · Heat Exchanger Fouling and Insufficient Heat Transfer · Waste-Heat Exchanger Finned · ★★
Gas-side ash deposition, K drop, waste-heat recovery down 30%
[Mechanism] Ash coats the fins and blocks heat transfer.
[Calculation] A 1 mm ash layer raises Rf, cuts K by 30%, and lowers recovered Q.
[Design Omission] No sootblowing and tight fin spacing, so ash accumulates.
1) Schedule steam sootblowing to clean fins (every shift / every 8 h); a 1 mm ash layer on fins raises Rf, cuts K by 30% and recovered waste heat by 30%, so sootblowing restores α and preserves recovery;
2) Widen fin spacing (replace dense fins with ≥6 mm pitch); narrow fins trap ash and resist cleaning, so wider spacing aids blowing and suppresses buildup;
3) Fit a draft-resistance alarm (alarm when draft resistance > design +15%); ash buildup raises draft resistance before recovery drops, giving early warning;
4) Pre-remove coarse ash at the inlet (cyclone / settling pre-collection); coarse particles dominate, so pre-collection cuts the load on the fins;
5) Keep gas velocity up to prevent settling (≥8 m/s); ash settles and hardens in low-velocity zones, so higher velocity reduces residence time;
6) Inspect fins on schedule (borescope / visual every two months); thickening ash worsens K and recovery loss, so data guides sootblowing;
7) Schedule ash-hopper discharge (timed ash removal to prevent plugging); accumulated ash plugs the path, so scheduled discharge keeps it clear;
8) Write sootblowing and fin spacing into the waste-heat procedure; the original design omitted sootblowing and used tight spacing, the root cause of ash buildup, so the procedure closes the loop.
GB/T 151-2014 Heat exchangers