E44-511 · Heat Exchanger Fouling and Insufficient Heat Transfer · Reboiler Vertical · ★★
Coked bottoms liquid bonding to walls, flow drop, weak evaporation, short run life
[Mechanism] Hot bottoms liquid cokes onto the wall.
[Calculation] A coke layer Rf=0.6 cuts K by 50%, lowers evaporation Q, and halves run life.
[Design Omission] No wall-temperature control and no scheduled decoking, so coking occurs.
1) Hold wall temperature below the coking threshold (wall temp ≤ the feed's thermal-cracking point); when wall temperature exceeds the coking point, heavy components condense and coke (Rf=0.6, K drop 50%, run life halved), so keeping wall temperature below the threshold suppresses coke deposition and preserves evaporation rate;
2) Schedule mechanical decoking (every 1500 operating hours); once the coke layer hardens it bonds strongly and hydraulic cleaning cannot remove it online, so periodic mechanical decoking restores flow area and heat transfer;
3) Raise flow velocity to prevent stagnation (≥ design upper limit); long residence time in low-velocity zones and wall heating promote coking, so higher velocity suppresses it;
4) Fit online K monitoring (alarm on 10% K drop); coking lowers K before flow drops, allowing early detection and planned decoking;
5) Pretreat feed to remove coking-prone components (filtration / hydrogenation); heteroatoms and heavy ends promote coking, so pretreatment cuts the coke source;
6) Optimize the operating cycle (reduce single-pass residence); coking limits run life and longer runs worsen it, so optimizing the cycle extends life;
7) Outlet temperature alarm (on exceeding setpoint); coking weakens the temperature rise, so the alarm prevents sudden upset;
8) Write temperature control and decoking into the reboiler procedure; the original design omitted wall-temperature control and decoking, the root cause of coking, so the procedure closes the loop.
GB/T 151-2014 Heat exchangers