Knowledge Base › Fluid Systems Error Case › Flue Gas Heat Exchanger Acid Dew-Point Corrosion

Flue Gas Heat Exchanger Acid Dew-Point Corrosion

E44-528 · Heat Exchanger Fouling and Insufficient Heat Exchange · Carbon-Steel Flue Gas Heat Exchanger · ★★

Problem Description

Wall temperature<acid dew point, acid corrosion pitting, air leakage, reduced heat exchange

Root Cause

[Mechanism] Flue gas acid dew-point attack corrodes holes in the wall.
[Calculation] A wall temperature <110℃ condenses acid, accelerating corrosion, causing pinhole leaks and lowering K.
[Design Omission] Wall temperature and sulfur content were not controlled, leading to acid attack.

Corrective Solution

1) Raise the wall temperature > the acid dew point (≥120℃) to prevent condensation; because sulfuric acid condenses when the wall temperature is <110℃, causing corrosive pinholes, air leakage and reduced K, raising the temperature prevents condensation and corrosion;
2) Coat the heat-transfer surface with an acid-resistant layer (enamel / alloy); because sulfuric acid corrodes holes and the coating blocks acid contact, coating extends service life;
3) Control fuel sulfur (low-sulfur / desulfurized fuel); because burning sulfur forms SO₃ that sets the acid dew point, controlling sulfur reduces acid;
4) Monitor for air leakage (oxygen content / differential pressure); because corrosion breakthrough causes air ingress and efficiency loss, leakage monitoring gives early detection;
5) Schedule soot blowing to prevent ash accumulation that promotes corrosion; because damp ash accelerates acid corrosion and buildup blocks passages, soot blowing keeps surfaces clean;
6) Control exhaust-gas temperature (> dew point +10℃); because low exhaust temperature condenses acid, temperature control prevents condensation;
7) Inspect for pinholes on schedule (borescope / thickness measurement); because corrosion progresses and holes enlarge into leaks, inspection guides patching;
8) Write wall-temperature and sulfur control into the flue gas heat exchanger procedure; because the original design omitted wall-temperature control and sulfur control, the root cause of corrosion, the procedure closes the loop.

Checklist

Reference

GB/T 151-2014 Heat exchangers