E44-538 · Heat Exchanger Fouling and Insufficient Heat Exchange · Graphite Electrolyte Cooler · ★★
Low-temperature crystallization blockage, reduced flow, rising bath temperature
[Mechanism] Low temperature causes salt crystals to adhere.
[Calculation] Controlling temperature < the crystallization point causes crystal adhesion, 30% blockage, and a 5℃ bath-temperature rise.
[Design Omission] Temperature was not controlled and no flushing was done, so crystallization occurred.
1) Keep temperature above the crystallization point (outlet temperature > salt crystallization point +5℃) to prevent crystallization; because controlling temperature below the crystallization point causes salt-crystal adhesion, 30% blockage and a 5℃ bath-temperature rise, temperature control prevents crystallization and restores passages;
2) Schedule flushing to remove crystals (hot-water flush every 8h, intensified flush at Δp>0.1MPa); because crystal buildup reduces flow area and differential pressure rises before full blockage, periodic flushing removes crystals;
3) Add a bath-temperature alarm (alarm at bath temperature > design +3℃); because crystallization lowers K first as a bath-temperature rise, well before full blockage, it gives early warning;
4) Raise flow velocity (≥1.2m/s) to prevent settling; because crystals settle and adhere in low-velocity zones and harden over time, higher velocity reduces residence time and suppresses settling;
5) Control concentration to prevent supersaturation (concentration ≤ saturation lower limit); because supersaturation causes crystal precipitation and adhesion, concentration control suppresses crystallization;
6) Use corrosion-resistant materials (graphite / titanium); because electrolyte attacks ordinary materials and corrosion pits promote crystallization, corrosion resistance extends life and suppresses crystallization;
7) Inspect crystal thickness on schedule (weekly thickness measurement / visual); because crystals thicken and worsen blockage and bath-temperature rise, quantifying it guides flushing;
8) Write temperature control and flushing into the electrolyte cooling procedure; because the original design omitted temperature control and flushing, the root cause of crystallization, the procedure closes the loop.
GB/T 151-2014 Heat exchangers