E44-1067 · Heat Exchanger Fouling and Insufficient Heat Transfer · Tubesheet · ★★★
Tubesheet leaks, cross-contamination, fouling
[Mechanism] Poor tube-to-tubesheet expansion / welding, joint loosening, and shell-to-tube-side cross leakage.
[Calculation] Expansion rate only 3% (should be 5–8%), 6 loose expanded joints, 3% shell-to-tube cross leakage, outlet water contaminated.
[Design Omission] Insufficient expansion, no expansion-rate verification, and no seal welding were provided.
1) Re-expand the tubesheet (expansion rate 6%); because looseness causes leakage and firm expansion seals it, this stops leakage;
2) Verify the expansion rate to 5–8% (actual 3%); because looseness causes leakage and rate verification ensures it, this seals the joint;
3) Add seal welding (use expansion plus welding); because leakage causes cross-contamination and welding seals and separates, this isolates the sides;
4) Perform a pressure test for leak detection (hold at 1.25 times design pressure); because leakage was never tested and direct measurement confirms no leak, this determines tightness from data;
5) Perform a helium leak test (leak rate≤1e-6 Pa·m³/s); because micro-leaks are hard to see and helium testing reveals them, this detects micro-leaks;
6) Install outlet water-quality monitoring (alarm on contamination); because leakage first shows up as contamination, this monitors leakage and gives early warning;
7) Control slow temperature ramp-up/down in operation (prevent loosening); because assembly transients cause leakage and controlling transients stabilizes it, this prevents leakage during operation;
8) Write firm expansion and rate verification into the process card; because the root cause of tubesheet leakage is insufficient expansion and lack of inspection, the process enforces control.
GB/T 151-2014 Heat exchangers