E44-784 · Piping Supports and Thermal Expansion · Sliding support · ★★
Sliding face rusted solid, displacement blocked, stress rise >50MPa
[Mechanism] An unlubricated or rusted sliding face blocks the thermal displacement.
[Calculation] Seizing blocks the displacement and raises the thermal stress >50MPa.
[Design Omission] The face was neither lubricated nor given clearance — causing the seizure.
1) Clean the sliding face and lubricate it (switch to heat-resistant lithium grease, 0.5mm thick): because the original rust seizure blocked the thermal displacement and raised the stress >50MPa, lubrication keeps it sliding;
2) Leave a sliding clearance to prevent binding (≥2mm in the sliding direction): because no clearance binds and leaving one allows movement, the clearance preserves displacement;
3) Verify the sliding face is flat (flatness ≤0.5mm/m): because a rough face binds and verifying flattens it, flattening cuts the resistance;
4) Apply an anti-corrosion layer (galvanize or use stainless steel on the sliding face): because rust binds and rust prevention protects, corrosion is prevented;
5) Monitor the sliding condition (displacement markers, alarm on binding): because gradual binding raises the stress and early awareness helps, sliding is monitored;
6) Guide the displacement (guide plates on both sides to limit offset): because offsetting binds and guiding straightens, the line is guided;
7) Run a thermal displacement test (raise the temperature and record the actual displacement against the calculation): because the original lack of testing led to the seizure and the test reveals the true displacement, the displacement is verified;
8) Write the lubrication and clearance into the assembly card: the original lack of lubrication was the root cause of the seizing, so assembly controls it and the support slides freely.
GB/T 17116.1-2018 Pipe supports and hangers