E44-790 · Piping Supports and Thermal Expansion · Bellows · ★★★

Problem Description

Bellows fatigue, cracking, leakage, life < design

Root Cause

[Mechanism] Cyclic displacement fatigues and cracks the bellows.
[Calculation] Displacement beyond the ± limit drops the cycle count < the design life, cracking and leaking the bellows.
[Design Omission] Fatigue was neither verified nor was the displacement limited — so it must be verified.

Corrective Solution

1) Verify the fatigue life (per EJMA, ≥ the design cycle count, with a 2× margin): because the original over-displacement drove the cycles < the life and cracked and leaked the bellows, verification raises the life;
2) Limit the displacement (guides to hold ± ≤ the nameplate value and prevent excess): because excess cracks and limiting protects, the displacement is limited;
3) Switch to a thicker bellows (increase the wall thickness by 0.3mm to raise the fatigue strength): because a thin wall cracks and a thicker one is stronger, the wall is thickened;
4) Add guide supports (≥4× pipe diameter at each end): because offsetting cracks and guiding straightens, the line is guided;
5) Monitor the wall thickness (measure it, alarm on thinning >10%): because gradual thinning brings cracking closer and early awareness helps, the thickness is monitored;
6) Avoid water hammer (add a relief valve against pressure surges): because hammering cracks and avoiding protects, hammering is avoided;
7) Control the temperature ramp rate (rise / fall ≤30℃/h): because a steep change cracks and a slow one keeps it under control, the ramp is controlled;
8) Write the fatigue verification and the displacement limits into the specification: the original lack of verification was the root cause of the fatigue, so the specification controls the design and gives a long life.

Checklist

Reference

GB/T 12777-2019 Metal bellows expansion joints

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »