E44-831 · Piping Supports and Thermal Expansion · Pipe Against Beam · ★★
Pipe rubbing against a beam, wall thinning, leakage
[Mechanism] Insufficient clearance between the pipe and the beam causes wear.
[Calculation] Contact causes wear and the wall thickness decreases >0.3mm per year.
[Design Omission] No clearance was left and none was checked — so clearance must be provided.
1) Leave clearance between the pipe and beam (leave ≥30mm of free clearance): because the original wear reduced the wall thickness >0.3mm per year and caused leakage, clearance prevents wear;
2) Check the pipe position to clear the beam (center the pipe axis, deviation ≤5mm): because contact causes wear and the check corrects it, the position is checked;
3) Add a protective pad to the pipe (line the beam side with a non-metallic material): because a hard surface wears and the pad protects it, the pad is fitted;
4) Weld a stop to prevent sliding (a stop block prevents displacement from touching the beam): because movement causes wear and the stop prevents it, the stop is welded;
5) Monitor the wear condition (measure the clearance / wall thickness, alarm on contact): because progressive wear brings leakage closer and early awareness helps, the wear is monitored;
6) Perform a position test (record the pipe-to-beam clearance in the hot state): because the original lack of testing left the wear undiscovered, the test reveals the true clearance, so the test is run;
7) Control thermal displacement (install compensation to absorb expansion and reduce contact): because expansion causes wear and control relieves it, displacement is controlled;
8) Write the clearance and position check into the assembly card: the original lack of clearance was the root cause of the wear, so assembly controls the work and the beam is not worn.
GB/T 17116.1-2018 Pipe supports and hangers