E44-837 · Piping Supports and Thermal Expansion · DN600 Crude-Oil Pipeline Pier · ★★
Pier spacing 12m with a design capacity of 80kN per pier; measured pipe sag 22mm, crack 0.3mm, settlement 15mm
[Mechanism] Pipe weight + contents + insulation load each pier; the soft-soil foundation settles when wet, and the unreinforced concrete lacks crack resistance and splits.
[Calculation] Load per pier N = pipe weight (62kg/m×12m) + contents (850kg/m³×0.283m²×12m) + insulation ≈150kN, exceeding the design 80kN and the foundation capacity of 120kPa; the pipe sag f=5qL⁴/384EI>20mm.
[Design Omission] The total weight was never calculated, the foundation capacity was never verified, and no reinforcement was provided for crack resistance.
1) Recalculate the total weight and set the pier spacing (derive the per-pier load from pipe + medium + insulation, and reduce the pier spacing from 12m to 8m): because the original per-pier load of 150kN exceeded the 80kN design value and caused cracking and settlement, the load is recalculated and reduced;
2) Verify the foundation bearing capacity (replace with 300mm crushed stone or treat until fk≥150kPa): because 15mm settlement of the soft soil made the pier crack diagonally, the foundation is stabilized and the pier is secured;
3) Use reinforced concrete (reinforcement ratio ≥0.2%, C30 or above): because unreinforced concrete has insufficient crack resistance and shows a 0.3mm crack, reinforcement is added for crack resistance;
4) Increase support density and reduce the span (change the pier spacing from 12m to 8m): because a large span raises the per-pier load to 150kN while denser supports bring it down to about 100kN, the per-pier load is reduced;
5) Inspect cracking and settlement (tap-check the crack width + level-survey the settlement, alarm at crack >0.2mm / settlement >10mm): because progressive cracking enlarges the pipe deflection and early detection can prevent it, cracking is inspected;
6) Perform a bearing test (load in stages up to 1.5 times the design value and check the settlement): because the original lack of testing left the cracking undiscovered, the test reveals the true bearing capacity, so bearing is tested;
7) Control the filling rate (fill in stages and continue only after the settlement stabilizes for 2h): because fast filling concentrates the instantaneous load and causes settlement while slow filling keeps it under control, the rate is limited;
8) Write the total weight, pier spacing and reinforcement into the foundation calculation sheet: the original design omission was the root cause of the cracking and settlement, and documenting it closes the loop, so calculation controls the design and the pier does not crack.
GB/T 17116.1-2018 Pipe supports and hangers