E44-045 · Insufficient Vessel Strength and Wall Thickness · Vacuum Buffer Tank · ★★
Evacuating to -0.08 MPa buckles and dents the tank; the roundness is out of tolerance and the tank cannot be used
[Instability] Under external pressure the critical pressure Pcr ∝ (t/D)²; when t/D is too small, Pcr < the operating negative pressure.
[Denting] Buckling wrinkles.
[Design Omission] The design did not follow external-pressure stability rules and no stiffening rings were added, so buckling caused denting.
1) Calculate the critical pressure Pcr for external-pressure stability and keep a margin, because Pcr ∝ (t/D)² and too small a t/D makes Pcr < the operating negative pressure of -0.08 MPa, causing buckling and denting, so Pcr must be calculated with allowance;
2) Install stiffening rings to improve buckling resistance, because the rings raise the effective t/D and increase Pcr, thereby stabilizing the tank;
3) Select the wall thickness per external-pressure design, because a thicker wall raises Pcr and resists denting, so thickness is chosen for external pressure;
4) Control the evacuation rate to prevent surge, because rapid evacuation causes a transient negative-pressure surge, so the rate must be controlled;
5) Control the tank roundness, because poor roundness makes the tank dent locally first, so roundness must be controlled;
6) Verify no denting by a negative-pressure trial evacuation, because the trial evacuation verifies stability, so it must be performed;
7) Provide vacuum relief protection, because excessive negative pressure is risky, so relief protection is required;
8) Incorporate external-pressure stability into vacuum tank design, because the original failure to check external pressure is the root cause of the buckling, so it must be checked in design.
GB/T 150.3-2011 Pressure vessels - Design