E44-196 · Insufficient Vessel Strength and Wall Thickness · Cryogenic tank (-40℃) · ★★★
No impact testing was performed; low-temperature brittle fracture caused leakage
[Brittle] With no impact test, the material toughness is insufficient and it embrittles at low temperature.
[Crack] Low-temperature brittle fracture.
[Design Omission] No impact-rated material selection and no low-temperature test, so it cracked.
1) Select low-temperature impact-qualified material for the cryogenic tank and perform Charpy testing, since the untested material has insufficient toughness and brittle-fractures at -40℃, thus impact-rated selection preserves toughness;
2) Use at reduced load per the design temperature, since exceeding the temperature embrittles it, thus controlling temperature;
3) Re-verify by low-temperature impact testing after welding, since the weld zone toughness changes, thus re-verification;
4) Avoid stress-concentrating structures, since concentration causes cracking, thus avoiding concentration;
5) Perform regular low-temperature inspections to prevent cracking, since cracking develops gradually, thus scheduled patrols;
6) Install leak monitoring and alarms, since cracking leads to leakage, thus monitoring and alarming;
7) Verify during commissioning that there is no cracking at low temperature, since the design requirement must be measured, thus confirming at delivery;
8) Include impact testing in low-temperature design, since the original lack of testing is the root cause of brittle fracture, thus the design must include it.
GB/T 150.1-2011 Pressure vessels General requirements