E45-199 · Grounding and Shielding · Outdoor Grounding Electrode · ★★
Three years after commissioning the grounding resistance rose from 3Ω to 15Ω, and the surge protection operated frequently
[Mechanism] In corrosive soil the grounding electrode's surface oxidises into a high-resistance layer, or corrosion at the joints raises the contact resistance; the overall grounding resistance climbs again, the drainage capability falls, and the residual voltage rises.
[Calculation] The corrosion layer raises the electrode-to-soil contact resistance 5× (3→15Ω); at a lightning current of 10kA the residual voltage climbs from 30kV to 150kV, which the SPD can hardly clamp.
[Design Omission] Neither a corrosion-resistant grounding electrode nor cathodic protection or periodic inspection was used.
① Corrosion-resistant electrode: use hot-dip galvanized steel or copper-clad steel grounding electrodes → corrosion-resistant
② Cathodic protection: add a sacrificial anode (magnesium block) → protects the electrode from corrosion
③ Joint protection: coat welded joints with bitumen → prevents rust-through
④ Periodic testing: measure the grounding resistance each year, R≤4Ω → catches a rise early
⑤ Resistance-reducing agent: fill a long-life agent around the electrode → stable contact
⑥ Redundant electrodes: add parallel grounding electrodes → R does not fail at a single point
⑦ Corrosion inspection: excavate to check the electrode body for corrosion → verify
⑧ Write grounding maintenance into the lightning-protection inspection routine → gate at the source
GB 50057-2010 Design code for protection of structures against lightning