E45-265 · Wiring and Terminals · Seaside Salt-Spray Site · ★
In the salt-spray environment the terminal surfaces corroded and formed insulating compounds; the contact resistance kept rising
[Mechanism] Chloride ions in the salt spray attack the metal terminals and form a mixed layer of conductive salts and oxides; the contact resistance rises as corrosion deepens and the signal gradually attenuates and distorts.
[Calculation] Corrosion of 0.05mm per year in salt spray raises the contact resistance from 0.02Ω to 0.3Ω in half a year; the extra drop in the 4-20mA loop makes the reading 2% low.
[Design Omission] No corrosion-resistant terminals, no protective coating, and no sealing.
① Corrosion-resistant terminals: use stainless-steel or tin-plated terminals → resist salt
② Protective coating: apply anti-corrosion paste to the contact surfaces → block salt
③ Sealed enclosure: use an enclosure rated IP54 or better → keep it out
④ Insulation measurement: check the contact resistance is stable → confirmation
⑤ Salt-spray test: verify by salt-spray testing → resistant
⑥ Periodic cleaning: remove salt deposits → early prevention
⑦ Corrosion inspection: check for no white or green rust → replace early
⑧ Write the anti-corrosion requirement into installation → control at the source
GB/T 2423.17-2008 Environmental testing for electric and electronic products - Part 2: Test methods - Test Ka: Salt mist