Knowledge Base › Electrical Sensor Error Case › Cable Cracking from Embrittlement at Very Low Temperature

Cable Cracking from Embrittlement at Very Low Temperature

E45-326 · Environmental Protection and Temperature/Humidity · Temperature Sensor · ★★

Problem Description

In a -40℃ cold-storage environment the PVC cable hardens and cracks; the copper strands break at the bend and the signal is interrupted

Root Cause

[Mechanism] Ordinary PVC has a glass-transition temperature of about -15℃; at -40℃ the jacket loses its elasticity and becomes brittle, and with equipment vibration microcracks form at the bends and grow until the copper core breaks.
[Calculation] PVC is rated to -15℃; an actual -40℃ is 25℃ lower, well past the embrittlement point. With the copper strands constrained by the brittle jacket, the bending strain concentrates and the fatigue life drops to one-tenth of that at room temperature.
[Design Omission] The selection did not check the minimum ambient temperature, and the jacket material's cold-resistance grade was insufficient.

Corrective Solution

① Material matching: for a -40℃ environment → choose a cold-resistant silicone or TPE jacket (rated to -60℃) that stays flexible at low temperature
② Bend control: keep the routing bend radius ≥10 times the cable diameter → reduce bending strain
③ Fixing and vibration damping: secure every 0.3m and leave a stress-relief loop → keep vibration from reaching the bend points
④ Redundant length: leave allowance for expansion and contraction → offset the tensile stress from low-temperature shrinkage
⑤ Joint protection: add cold-resistant heat-shrink tubing at the joints → prevent low-temperature cracking and moisture ingress
⑥ Probe selection: use a one-piece armored probe → no exposed embrittlement points
⑦ Low-temperature verification: run a -40℃ bend test before installation → confirm the jacket does not crack
⑧ Selection standardization: write the minimum ambient temperature into the mandatory items of cable selection → control at the source

Checklist

Reference

GB/T 5013.1-2008 Rubber insulated cables of rated voltages up to and including 450/750V