E45-360 · Environmental Protection and Temperature/Humidity · Photoelectric Sensor · ★★
Next to a welding station, a photoelectric switch's sheath is burned through by spattering weld slag; slag gets inside and blocks the light path, causing detection failure
[Mechanism] High-temperature weld slag spatters and strikes the sheath; once the plastic sheath is burned through, the spattered slag gets in and blocks the light path.
[Calculation] Weld slag exceeds 1000℃ while the plastic sheath melts at about 150℃, so it burns through instantly; the slag that gets in cuts the received light by 80% and the device fails.
[Design Deficiency] An ordinary plastic housing was used in the welding area, with no spatter protection.
① Metal shield: add a stainless-steel spatter shield → block weld slag
② High-temperature selection: choose a metal-housing, high-temperature model → resist burn-through
③ Quartz window: add a high-temperature quartz window at the lens → protect the light path
④ Location avoidance: install outside the spatter cone → less exposure to slag
⑤ Slag barrier: add a spatter baffle at the workstation → block flying slag
⑥ Regular cleaning: patrol and clear the slag from the lens → keep it transparent
⑦ Spatter verification: run a weld-slag spatter endurance test to confirm → data confirmation
⑧ Selection standardization: write the welding-spatter condition into the selection criteria → control at the source
GB/T 4208-2017 Degrees of protection provided by enclosures (IP code)