E45-361 · Environmental Protection and Temperature/Humidity · Level Sensor · ★★★
In the acid-mist environment of a chemical workshop, a level transmitter's terminals gradually oxidize and turn green, raising the contact resistance and causing signal attenuation and drift
[Mechanism] Chloride ions in the acid mist corrode the copper terminals and form green oxide; the resistive oxide layer increases the voltage drop in the signal loop.
[Calculation] Acid mist in the workshop raises the terminal contact resistance from 5mΩ to 200mΩ; the loop voltage drop attenuates the 4-20mA signal by 1.2%FS.
[Design Deficiency] The terminals were not gold-plated for corrosion protection, and the housing's sealing rating was too low to keep out the acid mist.
① Gold-plated terminals: choose corrosion-resistant gold-plated terminals → acid-mist resistance
② Fully sealed housing: choose an IP67 corrosion-resistant housing → block the acid mist
③ Potting isolation: epoxy-pot the terminal chamber → isolate chloride ions
④ Positive-pressure protection: fill the enclosure with dry nitrogen at a slight positive pressure → block ingress
⑤ Corrosion-resistant material: choose 316L or engineering plastic for the housing → corrosion resistance
⑥ Regular inspection: patrol for terminal oxidation and treat it promptly → early detection
⑦ Salt-fog verification: run an acidic salt-spray test to confirm → data confirmation
⑧ Selection standardization: write the acid-mist condition into the corrosion-protection selection criteria → control at the source
GB/T 2423.17-2008 Environmental testing for electric and electronic products - Salt mist test