E46-002 · Welding Process & Distortion · Thin-Plate Weldment · ★★
A 2mm thin plate was welded with an excessive current; the weld burned through into holes and leaked
[Mechanism] An excessive current makes the penetration exceed the plate thickness; the molten pool loses support and burns through into holes.
[Calculation] A current 30% above the process upper limit makes the penetration exceed the 2mm plate thickness; burn-through creates holes and leakage.
[Design gap] The current was not adjusted to the plate thickness.
① Select the current by plate thickness: choose a welding current that matches the thin-plate thickness to avoid an excessive current and burn-through
② Trial plate before welding: trial-weld on a test plate before production to set the parameters and ensure reliability
③ Control the welding speed: reduce the welding speed appropriately to keep the molten pool uniform and stable and avoid speed fluctuations
④ Weld with low parameters: use small-diameter electrodes and low parameters for thin plates so the penetration stays within the plate thickness
⑤ Add a backing: add a copper backing bar or backing strip behind the weld to support the molten pool and prevent burn-through into holes
⑥ In-process inspection: check for burn-through holes at any time during welding and correct them immediately
⑦ Test-plate section verification: section the trial plate before welding to confirm the parameters are suitable and verify the process by data
⑧ Standardize process: write the current upper limit and other parameters into the welding procedure specification (WPS), controlling at the source
GB/T 985.1-2008 Recommended groove for gas welding, shielded metal arc welding, gas-shielded welding and high-energy beam welding