E46-003 · Welding Process & Distortion · Low-Carbon Steel Structure · ★★
High-heat-input welding coarsened the grains in the heat-affected zone and lowered the impact toughness by 30%
[Mechanism] Excessive heat input makes the heat-affected zone stay at high temperature longer; the grains grow and the toughness drops.
[Calculation] A heat input above 28kJ/cm coarsens the grains and lowers the impact energy by 30%, exceeding the tolerance.
[Design gap] No upper limit was set for the heat input.
① Limit the heat input: keep the welding heat input within the process upper limit to avoid grain coarsening in the heat-affected zone
② Multi-layer multi-pass welding: use small-pass multi-layer multi-pass welding to reduce the heat input per pass and lower the heat
③ Increase the cooling rate: control the interpass temperature and raise the cooling rate appropriately to suppress grain growth
④ Choose fine-grain steel: prefer fine-grain steel grades to ensure weld toughness
⑤ Post-weld impact test: carry out a Charpy impact test after welding to measure the impact energy and detect a drop in toughness early
⑥ Re-qualify the welding procedure: re-qualify the welding procedure to ensure joint properties
⑦ Performance verification: confirm the toughness meets the requirement by the impact-test data
⑧ Standardize process: write the heat-input upper limit into the welding procedure specification (WPS), controlling at the source
GB/T 19866-2005 General principles for welding procedure specification and qualification