E46-004 · Welding Process & Distortion · Butt Weld · ★★★
The groove angle was small and the current insufficient, so the weld center lacked penetration; under load it cracked along the lack-of-fusion plane
[Mechanism] A large groove root face and a low current leave the root unfused; the incomplete penetration weakens the section.
[Calculation] Incomplete penetration reduces the effective thickness by 30%; the load stress rises and the joint cracks along the lack-of-fusion face.
[Design gap] The matching of the groove and the current was not checked.
① Groove by thickness: cut a suitable groove angle according to the plate thickness to ensure the root can be fully penetrated
② Match the current to the groove: adjust the root welding current to the groove size so the penetration reaches the root
③ Back-gouging: when welding from both sides, gouge the back and re-weld to ensure full-thickness fusion
④ Radiographic or ultrasonic inspection: inspect for incomplete penetration by RT or UT for early detection
⑤ Welding procedure qualification: section a test plate to confirm the root can be penetrated and fusion is ensured
⑥ In-process inspection: check the root bead shape during welding and correct any incomplete penetration promptly
⑦ Penetration verification: confirm the incomplete penetration has been eliminated by the NDT results
⑧ Standardize process: write the groove-to-current matching into the welding procedure specification (WPS), controlling at the source
GB/T 3323-2005 Radiographic examination of fusion-welded joints in metals