E46-008 · Welding Process & Distortion · Spot-Welded Thin Plate · ★★
The spot-weld spacing was too large; the middle of the overlap edge had incomplete fusion and cold welds, which separated under vibration
[Mechanism] Too large a spacing leaves no fusion nugget between the spot welds along the overlap; the middle cold-welds and separates.
[Calculation] A spacing above 30 times the plate thickness gives insufficient overlap strength; the joint separates under vibration.
[Design gap] The spacing was not checked against the plate thickness.
① Set the spacing by plate thickness: determine a reasonable spot-weld spacing from the plate thickness to ensure strength between the spots
② Trial weld and peel test: peel-test after a trial weld to confirm the nugget size is acceptable and the joint is sound
③ Control the electrode force: control the electrode force for good contact to ensure nugget formation
④ Sufficient current and time: use sufficient welding current and on-time to form an acceptable nugget
⑤ Periodic peel test: carry out destructive peel tests periodically for early detection of cold welds
⑥ In-process inspection: check for weld separation and correct it early
⑦ Strength verification: confirm the joint strength meets the requirement by the peel-test results
⑧ Standardize process: write the spacing and other parameters into the resistance-welding process specification, controlling at the source
GB/T 19867.1-2005 Welding procedure specification for resistance welding