E46-007 · Welding Process & Distortion · Stainless-Steel Vessel · ★★★
The weld was not annealed after welding; in a coastal environment stress-corrosion cracking occurred at the weld and leaked
[Mechanism] Residual stress plus a corrosive medium causes stress-corrosion cracking along the sensitized zone of the stainless steel.
[Calculation] Residual stress beyond the threshold propagates the crack tip in a Cl- environment and causes leakage within months.
[Design gap] No solution or annealing treatment was carried out.
① Post-weld solution annealing: solution-treat or anneal stainless steel after welding to relieve residual stress and prevent stress-corrosion cracking
② Choose ultra-low-carbon stainless steel: prefer ultra-low-carbon stainless steel such as 304L to improve resistance to sensitization
③ Control the chloride in the medium: reduce the chloride concentration of the service environment to slow the corrosion
④ Control the cooling rate: control the post-weld cooling rate to avoid sensitization and preserve the corrosion resistance
⑤ Penetrant inspection: inspect the weld for cracks by PT for early detection
⑥ Environmental isolation: apply a coating barrier on the weld surface to block the corrosive medium
⑦ Corrosion-resistance verification: confirm the corrosion resistance meets the requirement by the intergranular corrosion test
⑧ Standardize process: write the annealing requirement into the process specification, controlling at the source
GB/T 4334-2008 Corrosion of metals and alloys - Intergranular corrosion test of stainless steels