E46-006 · Welding Process & Distortion · Thick-Wall Vessel · ★★★
The stress was not relieved after welding; in service the vessel cracked along the weld at the stress-concentration point and leaked
[Mechanism] Welding residual stress combined with the service stress exceeds the yield of the material; a crack initiates at a defect.
[Calculation] Residual stress exceeding 50% of yield drives the total stress above the allowable value; the crack tip propagates and causes leakage.
[Design gap] No post-weld heat treatment was carried out to relieve stress.
① Post-weld stress-relief annealing: carry out annealing heat treatment after welding to relieve residual stress and reduce the cracking risk
② Weld peening: peen the weld surface to release stress and relieve residual stress
③ Control interpass temperature and cool slowly: control the interpass temperature and cool evenly to lower residual stress
④ Slow-cooling measures: cover with asbestos after welding to cool slowly and avoid cold cracking
⑤ Surface NDT: inspect for cracks by PT or MT for early detection
⑥ Stress measurement: measure the residual-stress level by the blind-hole method and correct it early
⑦ Stress-relief verification: confirm the residual stress has dropped into the safe range by the measured data
⑧ Standardize process: write the stress-relief heat-treatment requirement into the welding procedure specification (WPS), controlling at the source
GB/T 30583-2014 Post-weld heat treatment specification for pressure equipment