E46-012 · Welding Process & Distortion · Stainless-Steel Pipe · ★★★
The TIG weld was not purged with argon on the back; the root oxidized, suffered intergranular corrosion, perforated and leaked
[Mechanism] Without argon protection at the root, chromium oxidizes at high temperature; chromium depletion leads to intergranular corrosion and perforation.
[Calculation] Root oxidation lowers the Cr content, and intergranular corrosion perforates the wall and causes leakage.
[Design gap] No back-side argon purging was carried out.
① Back-side argon protection: purge with argon on the back during TIG welding to avoid root oxidation
② Use a trailing shield: protect the hot weld zone with a trailing shield to keep the weld color
③ Ensure argon purity: use argon with a purity of at least 99.99% to ensure the protection effect
④ Weld-bead color check: check the weld-bead color to judge the degree of oxidation and correct it early
⑤ Intergranular corrosion test: carry out an intergranular corrosion test for early detection of the tendency
⑥ Repair the oxidized section: repair heavily oxidized sections to restore the material
⑦ Protection verification: confirm good root protection by the color check
⑧ Standardize process: write the argon-purging requirement into the welding procedure specification (WPS), controlling at the source
GB/T 4334-2008 Corrosion of metals and alloys - Intergranular corrosion test of stainless steels