E46-013 · Welding Process & Distortion · Low-Alloy High-Strength Steel · ★★★
Welding continued with the interpass temperature above 200℃; cold cracks appeared in the heat-affected zone
[Mechanism] An excessively high interpass temperature degrades the heat-affected-zone structure; hydrogen accumulates and causes cold cracking.
[Calculation] An interpass temperature beyond the limit couples hardening with hydrogen cracking, propagating the crack tip.
[Design gap] The interpass temperature was neither measured nor controlled.
① Control the interpass temperature: keep the interpass temperature within the specified upper limit to stabilize the structure
② Infrared temperature measurement: monitor the interpass temperature with an infrared thermometer for early detection of overheating
③ Cool before resuming: when the interpass temperature is too high, pause and cool before welding again to avoid cracking
④ Preheat by carbon equivalent: preheat according to the carbon equivalent and control the cooling rate to cool slowly
⑤ NDT for cold cracks: inspect for cold cracks by NDT and correct them early
⑥ Control the material carbon equivalent: choose a material with a low carbon equivalent to reduce the hardening tendency
⑦ Temperature verification: confirm the temperature is controlled by the interpass-temperature records
⑧ Standardize process: write the interpass-temperature requirement into the welding procedure specification (WPS), controlling at the source
GB/T 19866-2005 General principles for welding procedure specification and qualification