Knowledge Base › Process and Assembly Error Case Study › No Back Gouging Causes Lack of Penetration

No Back Gouging Causes Lack of Penetration

E46-023 · Welding Process & Distortion · Double-Sided Welding · ★★

Problem Description

Without back gouging on a double-sided weld, the root had slag inclusions and lack of penetration, causing leakage

Root Cause

[Mechanism] Without back gouging the root of the first-side weld is not fused, leaving lack of penetration and slag inclusions at the root.
[Calculation] Without back gouging the root is not penetrated, reducing the effective thickness and causing leakage.
[Design gap] No back gouging was specified.

Corrective Solution

① Back gouging: back-gouge the reverse side of a double-sided weld to ensure root penetration
② Carbon-arc gouging: remove the weld root thoroughly with carbon-arc gouging
③ NDT for lack of penetration: use NDT to check for lack of penetration and detect it early
④ Repair-weld after gouging: repair-weld after gouging to ensure full-thickness fusion
⑤ Welding procedure qualification: verify penetration with a test plate to ensure quality
⑥ In-process inspection: check the root condition and correct early
⑦ Penetration-depth verification: confirm the root is penetrated by NDT
⑧ Standardize process: write the back-gouging requirement into the welding procedure specification (WPS), controlling at the source

Checklist

Reference

GB/T 3323-2005 Radiographic examination of fusion-welded joints in metals