Undersized Fillet Weld Leg

E46-022 · Welding Process & Distortion · Corner-Joint Part · ★★

Problem Description

A 5mm weld leg was undersized (8mm required), so the shear strength was insufficient and the joint came apart

Root Cause

[Mechanism] A weld leg smaller than designed gives an insufficient throat thickness, and the small shear area causes separation.
[Calculation] A 5mm weld leg gives an insufficient throat thickness, and the shear stress exceeds the allowable value, causing separation.
[Design gap] The weld-leg size was not checked.

Corrective Solution

① Adequate weld leg: make the weld leg no smaller than the designed 8mm to ensure strength
② Adjust parameters for a full leg: adjust the current and reduce the speed to make the leg full and reach the design size
③ Weld-leg measurement: measure the weld-leg size and correct early
④ NDT for defects: use NDT to check for defects and detect them early
⑤ Shear-strength check: check whether the shear strength meets requirements to ensure strength
⑥ Repair-weld undersized areas: repair-weld the undersized leg locations to restore strength
⑦ Size verification: confirm the requirement is met by weld-leg measurement
⑧ Standardize process: write the weld-leg size requirement into the drawing, controlling at the source

Checklist

Reference

GB/T 19418-2003 Arc-welded joints in steel - Quality classification of defects