E46-021 · Welding Process & Distortion · Fillet Weld · ★★
Excessive travel speed left the bead unfused to the base metal, and it separated under load
[Mechanism] Excessive travel speed gives insufficient heat input, so the edges are not fused.
[Calculation] A travel speed above the procedure gives insufficient heat input, and lack of fusion weakens the joint.
[Design gap] The travel speed was not controlled.
① Control travel speed: reduce the travel speed per specification to ensure enough heat input for fusion
② Ensure heat input: maintain sufficient welding heat input to ensure fusion
③ Sufficient current: use sufficient current to stabilize fusion
④ NDT for lack of fusion: use NDT to check for lack of fusion and detect it early
⑤ Test-plate sectioning: section a test plate to confirm good fusion and ensure quality
⑥ In-process inspection: check the weld bead formation and correct early
⑦ Fusion verification: confirm the lack of fusion has been eliminated by NDT
⑧ Standardize process: write the travel-speed requirement into the welding procedure specification (WPS), controlling at the source
GB/T 3323-2005 Radiographic examination of fusion-welded joints in metals