Uncorrected Arc Blow Causes Lack of Fusion

E46-025 · Welding Process & Distortion · Arc-Blow-Affected Weld · ★★

Problem Description

Arc blow deflected the bead toward the base-metal side, leaving lack of fusion and weakness

Root Cause

[Mechanism] Uneven magnetic fields cause arc blow, deflecting the heat to the base-metal side and causing lack of fusion.
[Calculation] Arc blow skews the weld width, and lack of fusion weakens the joint.
[Design gap] No demagnetization or position adjustment was done.

Corrective Solution

① Demagnetize before welding: demagnetize the workpiece before welding to correct the arc
② Symmetrical ground connection: connect the ground symmetrically to make the field uniform and correct the arc
③ Adjust the welding position: adjust the welding position to correct the arc
④ Use a short arc: use a short arc to stabilize the arc
⑤ NDT for lack of fusion: use NDT to check for lack of fusion and detect it early
⑥ In-process inspection: check for arc blow and correct early
⑦ Fusion verification: confirm the lack of fusion has been eliminated by NDT
⑧ Standardize process: write the demagnetization requirement into the welding procedure specification (WPS), controlling at the source

Checklist

Reference

GB/T 19866-2005 General principles for welding procedure specification and qualification