E46-026 · Welding Process & Distortion · Low-Alloy Steel · ★★★
Undried electrodes contained moisture, and the weld suffered hydrogen-induced delayed cracking and leakage
[Mechanism] Moist electrodes contain hydrogen, which enters the weld and enriches it, causing delayed cracking.
[Calculation] Hydrogen above the threshold causes diffusible-hydrogen cracking, leading to delayed cracking and leakage.
[Design gap] The electrodes were not dried.
① Dry the electrodes: dry the electrodes at 350℃ to lower the hydrogen content
② Keep them in a holding oven: after drying, keep them in a holding oven to prevent moisture pickup
③ Low-hydrogen consumables: use low-hydrogen electrodes to reduce the hydrogen source
④ Preheat and slow cooling: preheat before welding and cool slowly after to help hydrogen escape
⑤ Delayed NDT for cracks: perform delayed NDT after welding to check for hydrogen-induced delayed cracks and correct early
⑥ Post-weld heat treatment: apply stress-relief heat treatment after welding to reduce residual stress
⑦ Crack-prevention verification: confirm there are no delayed cracks by delayed NDT
⑧ Standardize process: write the drying requirement into the welding procedure specification (WPS), controlling at the source
GB/T 5117-2012 Covered electrodes for manual metal arc welding of non-alloy and fine grain steels