E46-029 · Welding Process & Distortion · Thin-Wall Tube · ★★
A 1mm thin-wall tube burned through into a hole during welding, and the medium leaked
[Mechanism] High current with no backing burns through the thin wall into a hole.
[Calculation] Excess current makes the penetration exceed 1mm, causing burn-through and leakage.
[Design gap] No backing rod was used and the parameters were not reduced.
① Insert a backing rod in the tube: insert a backing rod inside the thin-wall tube to support the molten pool and prevent burn-through
② Lower the parameters and use low current for thin walls: use low-current parameters for thin walls to avoid burn-through
③ Weld fast with brief arc stops: use fast welding with brief arc stops to lower the heat input
④ Stabilize shielding gas: keep the shielding gas and arc length stable to avoid porosity
⑤ Pneumatic leak test: perform a pneumatic test to check for leaks and detect them early
⑥ Repair burn-through: repair the burn-through locations to restore sealing
⑦ Burn-through-prevention verification: confirm there is no leakage by leak testing
⑧ Standardize process: write the thin-wall parameters into the welding procedure specification (WPS), controlling at the source
GB/T 985.1-2008 Recommended groove for gas welding, shielded metal arc welding, gas-shielded welding and high-energy beam welding