Repeated Weld Repairs Degrade Performance

E46-028 · Welding Process & Distortion · Critical Weld · ★★

Problem Description

Repairing the same spot 3 times degraded the heat-affected zone, lowering performance and causing leakage

Root Cause

[Mechanism] Repeated repairs repeat the thermal cycle and degrade the heat-affected zone, lowering performance.
[Calculation] Three repairs lower toughness by more than 30%, causing leakage under load.
[Design gap] The number of repairs was not controlled.

Corrective Solution

① Limit the number of repairs: repair the same spot no more than twice to ensure performance
② Completely remove the defect: completely remove the defect before repair and repair cleanly
③ Repair with the same procedure: repair using the same procedure as the original weld to stabilize quality
④ Preheat for repair: preheat before repair to avoid cracks
⑤ Full NDT after repair: perform full NDT after repair to detect problems early
⑥ Re-evaluate mechanical properties: re-evaluate the joint's mechanical properties to ensure strength
⑦ Repair verification: confirm the repair is acceptable by NDT
⑧ Standardize process: write the repair-count limit into the welding procedure specification (WPS), controlling at the source

Checklist

Reference

GB/T 19866-2005 General principles for welding procedure specification and qualification