E46-037 · Welding Process & Distortion · Stainless-Steel Weld · ★★★
Stainless steel with elevated sulfur and phosphorus hot-cracked along the grain boundaries and leaked
[Mechanism] Sulfur and phosphorus segregate to the grain boundaries, causing hot cracking at the final stage of solidification.
[Calculation] Excess sulfur and phosphorus raise hot-cracking susceptibility, causing intergranular cracking and leakage.
[Design gap] The sulfur and phosphorus content of the material was not controlled.
① Select low-sulfur, low-phosphorus material: select material with low sulfur and phosphorus content to improve hot-cracking resistance
② Low-impurity consumables: use low-impurity consumables to keep the deposited metal clean
③ Reduce heat input and weld fast: reduce heat input and weld fast to reduce segregation
④ NDT for hot cracks: use NDT to check for hot cracks and correct early
⑤ Check material composition: re-check the material's chemical composition to ensure purity
⑥ Welding procedure qualification: re-qualify to confirm the procedure is feasible and the properties are ensured
⑦ Crack-resistance verification: confirm hot-cracking resistance meets requirements by crack testing
⑧ Standardize process: write the sulfur and phosphorus control requirement into the specification, controlling at the source
GB/T 4334-2008 Corrosion of metals and alloys - Intergranular corrosion test of stainless steels