E46-036 · Welding Process & Distortion · Precision Frame · ★★★
Release of post-weld residual stress shifted the frame's hole positions by more than 0.1mm, out of tolerance
[Mechanism] Release of post-weld stress slightly deforms the precision part and shifts the hole positions.
[Calculation] Stress release shifts the position by more than 0.1mm, putting assembly out of tolerance.
[Design gap] Machining was done without prior stress relief.
① Stress-relieve after welding first: apply stress-relief treatment after welding to stabilize the shape
② Weld before machining: sequence welding before machining to avoid distortion
③ Natural aging: apply natural aging to stabilize dimensions and reduce stress release
④ Separate roughing and finishing: separate rough machining from finish machining to ensure accuracy
⑤ Re-measure before machining: re-measure the dimensions before machining and correct early
⑥ Clamp securely during machining: clamp securely during machining to avoid shifting
⑦ Dimension verification: confirm dimensions meet requirements by CMM measurement
⑧ Standardize process: write the stress-relief sequence into the process, controlling at the source
GB/T 19866-2005 General principles for welding procedure specification and qualification