Worn Spot-Welding Electrodes Cause Cold Welds

E46-039 · Welding Process & Distortion · Spot Welder · ★★

Problem Description

With worn electrodes the contact area was small, and the spot welds were cold and came apart

Root Cause

[Mechanism] Worn electrodes reduce the contact area and raise the current density, producing small nuggets and cold welds.
[Calculation] Worn electrodes reduce the contact area, giving an undersized nugget and a cold weld.
[Design gap] The electrodes were not replaced periodically.

Corrective Solution

① Replace and dress electrodes periodically: replace or dress the electrodes periodically to ensure an adequate contact area
② Dress the electrode tip shape: dress the electrode tip shape to ensure proper contact
③ Control electrode force: control the electrode force to ensure nugget formation
④ Periodic peel test: perform peel tests periodically to detect cold welds early
⑤ Calibrate the current: calibrate the welding current to stabilize the nugget
⑥ In-process inspection: check electrode wear and correct early
⑦ Strength verification: confirm the joint strength meets requirements by peel test
⑧ Standardize process: write the electrode-replacement requirement into the specification, controlling at the source

Checklist

Reference

GB/T 19867.1-2005 Welding procedure specification for resistance welding